Hey froghunter, glad to hear you're gonna save that old girl. As far as the rust pitting, the fix is simple but a little time consuming. First, wipe er' down with some sort of paint prep (thinner works). Then spray it with one coat of metal etching primer. After the etcher dries, spray on two to three coats of high build primer. Spray it on pretty thick. All of this stuff is available in a spray can at most auto parts stores. Try to stick with the same brand. After that flashes off, lightly mist it with a contrasting color. Get a rubber sanding block, an ice cream pail full of warm water with a drop of dishsoap, some 300 grit and some 600 grit wet/dry paper. Sand in a crosshatch pattern, dipping the block/paper in the water frequently, until the contrasting mist dissappears, or you start to get back to bare metal. The mist will reveal the spots that are still low. It's up to you haw far you want to go. One prime/block session should take care of most if not all of the pitting. If not, you could spray the new bare metal areas with etcher and repeat the process again. Or, you could buy a tube of 3m spot putty/glaze, and fill the remaining low spots with that using a bondo spreader. This stuff is meant to go over primer, but it is not meant to fill anything more than paper thick, or go onto bare metal. Whatever you decide to do, finish by wet sanding with the 600 or 800 grit paper before you finish with color. It sounds worse than it is. Don't hesitate to ask if you have a question. All of this stuff is pretty cheap. You should'nt need more than one can of etcher and at most two cans of high build. Total investment of maybe 30 bones? The spot putty is kinda spendy, like twenty bucks for a big tube, but it is good stuff. Good luck!
-Jared