Several ways to clean the tank including some radiator shops. If you have much pitting I suggest that no further loss of metal. After it's clean use one of the tank liner coatings like POR 15. Or you can install a filter inside the tank in the fuel valve inlet Check the HOW TO Forum for some ideas. JMHO StanWhat process do you recommend to remove light rust with some pitting from a cub gas tank? Also, what are your thoughts about tank linings/coatings?
I have had great success with Muriatic Acid, it’s cheap and works quickly. But you have to be cautious and wear protective gloves and a face shield.What process do you recommend to remove light rust with some pitting from a cub gas tank? Also, what are your thoughts about tank linings/coatings?
Thanks - I bought a gallon of muriatic acid, but I'm not sure about how much to dilute it, and how long to let it soak - any recommendations?I have had great success with Muriatic Acid, it’s cheap and works quickly. But you have to be cautious and wear protective gloves and a face shield.
I have diluted it 1 to 1, plugged outlet in the gas tank then 10 minutes on the bottom, then rotate to the side for 10 minutes, then rotate to the opposite side for 10 minutes. I usually don’t do anything to the top unless it’s really bad because it’s gonna leak out the gas cap some so be prepared to catch what comes out If you do the top.Thanks - I bought a gallon of muriatic acid, but I'm not sure about how much to dilute it, and how long to let it soak - any recommendations?
That's what I was talking about when I said no further loss of metal. It can be fixed but it just adds to the magnitude of the problem. My suggestion is to wash the tank clean with detergent and hot water, dry with compressed air or alcohol then coat the interior with OSPHO or a similar rust stop product and install a standup filter screen in the fuel shutoff valve. That will solve the rust problem and prevent any trash from leaving the tank. JMHO StanIf you have pitting inside or outside the tank, be careful. The sheet metal is not very thick and you could end up with a bunch of pin holes using the acid.
Regular household vinegar will work also, it just takes it longer. Any of the acid products will eventually eat away more of the metal, that's why the baking soda wash is so important. It neutralizes the acid by changing the ph. That's the main reason that I posted the method above about sealing the surface with a rust prevention product to encapsulate the surface. JMHO StanI have used cleaning vinegar (home depot ~30% acid) just because I was a little concerned about working with muriatic acid. I let it sit with some rotation for about a week. I then rinsed with water and baking soda and then water, and then sprayed the inside with fluid film lubricant.
I have not used the Evaporust product but I've used OSPHO for more than 25 years with exceptional results. If the metal is wire brushed or otherwise cleaned of any loose surface rust then coated with OSPHO, it will turn dark. Heavy rusted metal will have a powder like material which will wipe away with a cloth or brush but is not necessary to remove if the metal is to be painted after OSPHO treatment. Example: rusty bolts, nuts, wrenches, etc that is given a vinegar bath for a few days then flushed with plenty of water and air dried will have the dark color where the rust was located. Paint or otherwise coat as desired. I have a LP gas tank that the outside surface was done more than 20 years ago and it's still in good condition. JMHO StanI have used the muriatic acid approach as well and followed with Redkote.
The next time I do that, I think I will go the safer route and use Evaporust. Way safer for me, for my work environment (ie, the yard) and the tank itself. It won’t damage the metal. Over night will probably be sufficient, but leave it in as long as you like. The only thing that will happen is the bare metal will turn a dark gray.
I don’t believe this would impact using a lining like POR 15 or Redkote, but I don’t know for sure.
However, thinking back to the couple of things that I have used this on before, it may not need the lining? Once things came out of the liquid, they did not flash rust. I don’t think that the dark color is really any kind of protective coating, but it certainly does not leave the exposed steel as raw and eager to react as the acid does.