jb weld and paint

ReTractor

Well-known member
not sure where to post this one....
I used JB weld to do a repair on an item (not a tractor part, not even close) that I then painted with International Harvester Red-Rustoleum Farm Equipment paint. Anywhere the paint touched original metal it dried fine. The only place it seems to be not curing/drying is on JB weld where there is fairly thick build- maybe 3/16-1/4" thick.:o There are other areas with JB Weld where it is not that thick and I don't have an issue with drying there. I'm asking here since I believe that many have used JB weld and may have some insight. Any ideas what might be going on? Will it dry completely at some point? It's been more than 24 hours now and still not feeling completely dried.
 
If the JB Weld is applied thickly it will take some time to cure out completely. Let it set a week and then paint it.
 
JB can be accelerated by heat, they recommend waiting an hour before applying the heat, but I typically will set it under a halogen work lamp immediately if it won't flow out of the area, I wait the hour if I want it to stay put. The heat accelerates the curing, still good to let it take some time, it will eventually stop smelling like jb weld.
 
Back
Top